Arcast produces fine titanium superalloy powder

May 8, 2019

News
May 8, 2019

Arcast Inc., Oxford, Maine, USA, reports that it has successfully produced a titanium superalloy powder with an as-atomised D50 of 20 µm, with narrow size distribution and with little-to-no oxygen pick-up. The alloy was produced using Arcast’s proprietary atomising process.

Arcast’s process consumes relatively little gas and has zero risk of ceramic/oxide contamination, the company states, making it possible to process metal alloys which other methods cannot. Powders produced by this method can be used in Additive Manufacturing, Metal Injection Moulding and other Powder Metallurgy processes.The production of powder by this process also does not require specialist feedstock.

Arcast stated that the new alloy is now being produced in significant quantities. With its growing capacity to produce as-atomised, advanced titanium alloys (along with other challenging metal alloys) from a range of low-cost feedstock, Arcast states that it can offer a complete solution for Additive Manufacturing, Metal Injection Moulding and other Powder Metallurgy markets.

News
May 8, 2019

In our latest magazine…

Download PDF

Extensive metal powder and Powder Metallurgy news coverage, plus the following exclusive deep-dive articles and reports:

  • GKN Powder Metallurgy targets sustainable and resilient regional NdFeB magnet production
  • The chemistry of LiFe: The rise of LFP batteries and what it means for the iron powder industry
  • Driving sustainable innovation: HIP 2025 explores the strategic potential of Hot Isostatic Pressing
  • High-precision press solutions for permanent magnets in EVs and green energy generation
  • Powder2Powder: A closed-loop solution for high-value metal powder recycling
  • Reducing defects and energy use in Hot Isostatic Pressing: A data-driven approach to degassing

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of Metal Powder Technology, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join 5,000+ other industry professionals – follow us online

Discover our magazine archive…

The free-to-access Metal Powder Technology magazine archive offers unparalleled insight into the world of metal powder from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of Metal Powder Technology magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • HIP Services
  • AM Machines
  • Consulting & toll sintering
View online
Share via
Copy link