Elementum 3D brings NASA’s GRX-810 high-temperature superalloy to commercial availability

December 3, 2024

MaterialsNews
December 3, 2024
Elementum 3D has announced the commercial availability of GRX-810 (Courtesy Elementum 3D)
Elementum 3D has announced the commercial availability of GRX-810 (Courtesy Elementum 3D)

Elementum 3D, based in Thornton, Colorado, USA, has announced the commercial release of GRX-810, an additively manufacturable nickel cobalt chromium oxide dispersion strengthened (ODS) superalloy. First developed by Dr Tim Smith and team at NASA Glenn Research Center, the metal powder is now commercially available from Elementum 3D through a co-exclusive licensing agreement.

Elementum 3D shipped the first commercially produced GRX-810 to a customer in October and has the capacity in place to produce 1.5 tons per week.

“I’m proud of how the Elementum 3D team rallied to quickly bring NASA’s GRX-810 alloy to market. Development of a qualified manufacturing process to mass produce GRX-810 in six months is a testament to our ability to turn concepts into reality,” said Dr Jacob Nuechterlein, Elementum 3D CEO and Founder.

THE WORLD OF METAL POWDERS TO YOUR INBOX
Subscribe to our weekly newsletter
Register now

This achievement is welcoming news for engineers eager to take advantage of the exceptional material properties offered by GRX-810, combined with the design complexity enabled by Additive Manufacturing. Potential breakthroughs enabled by this additively manufacturable material include lighter and thinner engine parts, increased fuel efficiency, lower operating costs, increased durability, and higher operating temperature capability. Manufacturers in aerospace, space, and energy are particularly interested in this high-temperature superalloy material.

The chart provides typical performance data from NASA and Elementum 3D for Laser Beam Powder Bed Fusion manufactured GRX-810. As can be seen, the material offers superior high temperature creep and oxidation resistance compared to other available AM superalloys (Courtesy Elementum 3D)
The chart provides typical performance data from NASA and Elementum 3D for Laser Beam Powder Bed Fusion manufactured GRX-810. As can be seen, the material offers superior high temperature creep and oxidation resistance compared to other available AM superalloys (Courtesy Elementum 3D)

GRX-810 is designed to offer excellent mechanical strength and exceptional creep performance at high temperatures. As Elementum 3D explains, creep life is the duration a material can withstand continuous stress at high temperatures without failure. Enhanced creep performance can directly lead to longer part life and higher operating temperature and load capability.

GRX-810 is reported to result in 1,000-fold better creep resistance with a two-fold increase in strength and oxidation resistance, compared to other additively manufactured superalloys.

www.elementum3d.com

MaterialsNews
December 3, 2024

In our latest magazine…

Download PDF

Extensive metal powder and Powder Metallurgy news coverage, plus the following exclusive deep-dive articles and reports:

  • GKN Powder Metallurgy targets sustainable and resilient regional NdFeB magnet production
  • The chemistry of LiFe: The rise of LFP batteries and what it means for the iron powder industry
  • Driving sustainable innovation: HIP 2025 explores the strategic potential of Hot Isostatic Pressing
  • High-precision press solutions for permanent magnets in EVs and green energy generation
  • Powder2Powder: A closed-loop solution for high-value metal powder recycling
  • Reducing defects and energy use in Hot Isostatic Pressing: A data-driven approach to degassing

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of Metal Powder Technology, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join 5,000+ other industry professionals – follow us online

Discover our magazine archive…

The free-to-access Metal Powder Technology magazine archive offers unparalleled insight into the world of metal powder from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of Metal Powder Technology magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • HIP Services
  • AM Machines
  • Consulting & toll sintering
View online
Share via
Copy link